1-4% by weight of total formula,should not exceed 4%,mix with other materials and extrude.Through extruder extrusion, please control the extrusion temperature uniformity, gloss decreases with the increase of the dosage.
Reference formulation: Raw material | 1 | 2 | Epoxy | 30.5 | 25.6 | 50/50 Polyester | 24.5 | -- | 60/40 Polyester | -- | 29.4 | L88 Leveling Agent | 1 | 1 | L701 Gloss Enhancer | 1 | 1 | L307 Benzoin | 0.5 | 0.5 | Titanium Dioxide+ Barium Sulfate | 38 | 38 | pigment | 0.5 | 0.5 | L2036 Matting Agent | 4 | 4 | Total | 100 | 100 |
|
|
| Extrude Temperature | 100-110℃ | 100-110℃ | Baking Condition | 190*15mins | 190*15mins | Gloss | 6 | 8 |
Notice: ● We don't suggest add accelerator to improve the mechanical properties in formulation,cause it may lead to gloss increase and floor worse,small test is recommended at first. ● Some matting wax powders may bring adverse effect on the system.We suggest to make sure the compatibility between matting wax powder and matting agent by experiments. ● Baking temperature has a certain effect on gloss stability. Lower baking temperature may lead to higher gloss.We suggest that stable baking conditions be ensured. ● The system is highly interfered by 68 matting agent,pls avoid cross use. ● The storage performance of semi chemical system is relatively good, but attention should also be paid to storage time control. ● Too many dosage will increase the gloss,pls do small test at first.
Dosage and gloss (curve)

|